1905: exhibits by F. W. Harbord
Find out more about this exhibition
List of all exhibits from the catalogue for this exhibition:
| Exhibit no. | Exhibitor | Exhibit title | Section | Picture | Catalogue |
|---|---|---|---|---|---|
| 544 | F. W. Harbord (Alfred Campion) |
0.30% Carbon Steel. Cast in sand. Untreated. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 545 | F. W. Harbord (Alfred Campion) |
0.30% Carbon Steel. Cast in sand. After annealing. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 546 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. As rolled, x 150 diam. Enlarged 3 diam. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 547 | F. W. Harbord (Alfred Campion) |
0.947 % Carbon Steel. As rolled, x 1,500 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 548 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated to 820° C.; slowly cooled, x 150 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 549 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated to 820° C.; slowly cooled, x 1,500 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 550 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated 820° C.; quenched in water at 15° C., x 1,500 diameters. Enlarged 3 diameters. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 551 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated 820° C.; quenched in water at 15° C., x 150 diameters. Enlarged 3 diameters. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 552 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated 820° C.; quenched in oil at 15° C., x 1,500 diameters. Enlarged 3 diameters. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 553 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated 820° C.; quenched in oil at 15° C., x 150 diameters. Enlarged 3 diameters. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 554 | F. W. Harbord (Alfred Campion) |
0.947% Carbon Steel. Heated 820° C.; quenched in oil at 15° C., reheated 650° C.; slowly cooled, x 150 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 555 | F. W. Harbord (Alfred Campion) |
0.35% Carbon Steel. Heated 1,100° C. 6 hours: slowly cooled, x 150 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 556 | F. W. Harbord (Alfred Campion) |
0.35% Carbon Steel. As rolled, x 150 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 557 | F. W. Harbord (Alfred Campion) |
0.65% Carbon Steel. As rolled, x 150 diameters. Enlarged 3 diameters. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 558 | F. W. Harbord (Alfred Campion) |
0.65% Carbon Steel. Heated 1,100° C. 6 hours; slowly cooled, x 150 diameters. Enlarged 3 diameters. |
Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 559 | F. W. Harbord (Alfred Campion) |
Outside of 4-in. bar. 0.50% carbon steel as rolled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 560 | F. W. Harbord (Alfred Campion) |
Average of 4-in. bar. 0.50% carbon steel as rolled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 561 | F. W. Harbord (Alfred Campion) |
Centre of 4-in. bar. 0.50% carbon steel as rolled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 562 | F. W. Harbord (Alfred Campion) |
Centre of 4-in. bar. 0.50% carbon steel heated 940° C. half and hour; slowly cooled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 563 | F. W. Harbord (Alfred Campion) |
Outside of 6-in. forged bar. 0.35% carbon heated 760° C. half an hour; cooled over week-end. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 564 | F. W. Harbord (Alfred Campion) |
Average of 6-in. forged bar. 0.35% carbon heated 760° C. half an hour; cooled over week-end. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 565 | F. W. Harbord (Alfred Campion) |
Centre of 6-in forged bar. 0.35% carbon heated 760° C. half an hour; cooled over week-end. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 566 | F. W. Harbord (Alfred Campion) |
Outside 6-in. forged bar. 0.585% carbon steel heated to 900° C.; slowly cooled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 567 | F. W. Harbord (Alfred Campion) |
Average 6-in. forged bar. 0.585% carbon steel heated to 900° C.; slowly cooled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 568 | F. W. Harbord (Alfred Campion) |
Centre 6-in. forged bar. 0.585% carbon steel heated to 900° C.; slowly cooled. | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 569 | F. W. Harbord (Alfred Campion) |
Ferrite | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 570 | F. W. Harbord (Alfred Campion) |
Pearlite | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 571 | F. W. Harbord (Alfred Campion) |
Cementite, x 150 diameters | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 572 | F. W. Harbord (Alfred Campion) |
Cementite, x 1,500 diameters | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 573 | F. W. Harbord (Alfred Campion) |
Cementite and Pearlite | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 574 | F. W. Harbord (Alfred Campion) |
Martensite | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page | |
| 575 | F. W. Harbord (Alfred Campion) |
Austenite | Loan Collection of British Technical and Scientific Photographs from the St. Louis International Exhibition of 1904 | catalogue page |